How to better press semi-coke powder
Category:
Company News
Author:
Source:
Release time:
2021-01-21
In the second step, pulverized coal with particle size less than 1mm is heated to 500 ℃ ~ 700 ℃ by a heating device; The third step is to crush bituminous coal by a crusher to control the particle size less than 1mm. In the fourth step, bituminous coal with particle size less than 1mm is heated to 150 ℃ ~ 380 ℃ by a heating device. In the fifth step, the pulverized coal in the second step and bituminous coal in the fourth step are fed into a mixing device at 50% ~ 80%:50% ~ 20% mixing; The sixth step is to send the mixture of the fifth step into a roller press with an online pressure of 150kn/cm ~ 250kN/cm for pressing, and the particle size after forming is controlled at 10mm ~ 80mm; Step 7: Send the product pressed and formed in step 6 to a stuffing machine at a stuffing temperature of 450 ℃ ~ 900 ℃ and a stuffing time of 3~8 hours; Step 8: send the stuffed product in step 7 to a cooling device to cool to room temperature.